This might appertain to railway modellers or Dihorrama modellers more than boaters in general, but thought you might like to know.
The other day I was trying to get the dregs out of two bottles of 2 part epoxy so put them into boiling water to soften the glue up.
After a few minutes I mixed it in a small margerine tub.
As soon as the mix reacted chemically,(within a minute or so of mixing.not immediatly) it ballooned up , fizzed away for a few seconds and then set in a conglomeration that looked like a mix between chalk, moonrock and pumice stone, and then went hard, retaining that shape.
I tried it again with some newer stuff and it did the same.
In the end it looked as though a large lump of rock, and I thought it could be usefull for open cargo well decks, scenery and such, as it has the consistency of rock without any weight.
Has anyone else come accross stuff that could be used for detailing by chance or mistake.